Gray iron | Ductile iron | Low carbon steel castinhg | Low Alloy steel casting | |
Degradation of tensile strength at 750°F | <15% | <15% | <15% | <15% |
Degradation of yield strength | - | <15% | <15% | <15% |
Degradation of elongation strength at 750°F | - | <15% | <15% | <15% |
Degradation of resistance at 1100°F | <50% | <50% | <90% | <50% |
Degradation of resistance at 1300°F | >75% | >75% | >95% | >80% |
QI | < 500 | 38000 | 55000 | 50000/85000 |